英文: Abstract: In this paper,through the hydrogen-filling test for the kovar alloy of austenite under fixed load,the kovar alloy hydrogen brittleness sensitivity is measured its feature on hydrongen brittleness fracture is studied,and the way of solving the fr
中文: 文摘:通过对面心立方奥氏体的可伐合金衡载荷充氢试验,测试了其氢脆敏感性并研究了氢断裂特征,提出了解决可伐合金脆断的方法。
更详细...
英文: Combining with the results of implant test, the conclusion that the main reason of dropping the strength of Austenite zone is the micro-crack located in the tip of flake graphite and Marten site is drawn.
中文: 结合插销试验结果提出了马氏体相变过程中,在片状石墨尖端及马氏体组织中造成的微裂纹是奥氏体区强度下降并进而在外力作用下断裂的主要原因。
更详细...
英文: Its austenite has two types of morphologies: one type is the austenite which is existing between the acicular ferrite and has approximately equiaxial block shape; another type is the austenite which is existing inside the acicular ferrite and has thin sli
中文: 其奥氏体有两种形态:一种是存在于针状铁素体之间的近似于等轴形的块状奥氏体;一种是存在于针状铁素体之内的薄片形奥氏体。
更详细...
英文: J.K.Chen and W.T.Reynolds Jr., Effects of Alloying Elements upon Austenite Decomposition in High Strength Low Alloy Steels, 1993 Materials Week, Pittsburgh, PA.
中文: 陈贞光,李至隆,「碳锰钢碳氮内耗峰之分解」,1998年中华民国材料科学年会,台北。
更详细...
英文: So far as the grain size order of magnitude is concerned, the thickness of the acicular ferrite is about 200nm, while the thickness of the austenite existing inside the ferrite is only several nm to 10 nm.
中文: 从晶粒尺寸数量级来说,针状铁素体的厚度约为200纳米,而铁索体内奥氏体的厚度仅为几到10纳米数量级。